Table 6 Means and standard deviations of fracture resistance (N) of different ceramics with oral hygiene aids type.
Ceramic type | Oral hygiene aids type | Fracture resistance (N)Mean (SD) | Overall fracture resistance (Newton) | P |
---|---|---|---|---|
IPS e.max CAD | Miswak toothpaste | 836.58 (111.10) | 829.21±101.79 | 0.051 |
Miswak mouthwash | 771.80 (80.84) | |||
Miswak stick | 879.24 (113.42) | |||
Vita Suprinity | Miswak toothpaste | 346.64 (59.23) | 340.63±55.93 | 0.241 |
Miswak mouthwash | 331.27 (52.40) | |||
Miswak stick | 343.98 (54.54) | |||
Vitablocs Mark II | Miswak toothpaste | 304.29 (18.01) | 312.65±19.33 | 0.198 |
Miswak mouthwash | 302.25 (11.75) | |||
Miswak stick | 331.40 (28.23) | |||
* Significant difference at ≤0.05. |